Solution to surface crack of plastic shell of power supply

Release time:2023-05-06

Plastic shell of power supplyDuring injection molding, cracks formed by surface cracking are called cracks. We solve this problem through fault analysis and troubleshooting.


1. Residual stress is too high

In terms of mold design and manufacturing, the direct gate with small pressure loss and high injection pressure can be used, and the forward gate can be changed into multiple needle point gates or side gates to reduce the gate diameter. When designing the side gate, the convex gate that can remove the broken part after forming can be used.

From the perspective of process operation, reducing the injection pressure is a relatively simple method to reduce the residual stress, because the injection pressure is in direct proportion to the residual stress. The temperature of the barrel and the mold should be appropriately increased, the temperature of the melt and the mold should be reduced, and the cooling time and speed of the parison in the mold should be controlled, so that the oriented molecules have a longer recovery time.


2. Residual stress concentration caused by external force

Generally, this kind of fault always occurs around the ejector rod. In case of such failure, the ejector shall be carefully checked and calibrated, and the ejector rod shall be set at the position with large demoulding resistance such as boss and stiffener. If the number of ejector pins cannot be expanded due to the limitation of pushing area, the method of small area and multiple ejector pins can be adopted. If the mold cavity demoulding slope is not enough, the surface of the plastic shell of the power supply will also be scratched to form wrinkles.

圖片3-1.png


3. There are differences in thermal expansion coefficients between raw materials and metal inserts

Metal inserts should be preheated, especially when cracks appear on the surface of the plastic shell of the power supply at the initial stage of startup, most of which are caused by the low temperature of the inserts.

In addition, in the selection of insert materials, try to use materials with linear expansion coefficient close to resin characteristics. When selecting raw materials for molding, high molecular weight resins should be used as much as possible. If low molecular weight molding raw materials must be used, the thickness of plastic around the insert should be designed to be thicker.


4. Improper or impure selection of raw materials

Practice shows that low viscosity loose resin is not easy to crack. Therefore, in the production process, appropriate molding raw materials should be selected according to the specific situation. During operation, pay special attention not to mix polyethylene, polypropylene and other resins together, which is easy to produce cracks. During the molding process, the release agent is also a foreign matter for the molten material. If the amount is improper, it will also cause cracks, so the amount should be reduced as much as possible.


5. The structural design of the plastic shell of the power supply is poor

The sharp corners and cracks in the structure of the plastic shell of the power supply are easy to produce stress concentration, resulting in cracks and cracks on the surface of the plastic shell of the power supply. Therefore, the outer and inner corners of the plastic shell shape structure of the power supply should be made into an arc with the largest radius as far as possible. The experiment shows that the best transition arc radius is that the ratio of arc radius to wall thickness at the corner is 1:1.7.


6. The cracks on the mold are reflected on the surface of the plastic shell of the power supply

In the process of injection molding, due to the repeated action of injection pressure on the mold, fatigue cracks will occur at the edges with acute angles in the cavity, especially near the cooling hole.

When the cracks on the surface of the mold cavity are reflected on the surface of the plastic housing of the power supply, the cracks on the surface of the plastic housing of the power supply always appear continuously in the same shape and position. When such cracks appear, immediately check whether the cavity surface corresponding to the cracks has the same cracks. If the crack is caused by reflection, the mold should be repaired by machining.

Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
主站蜘蛛池模板: a级大胆欧美人体大胆666| 午夜精品久久久久久久2023| 天码欧美日本一道免费| 久久精品中文字幕无码绿巨人| 亚洲一区二区三区无码国产| 肉大捧一进一出免费视频| 日韩人妻高清精品专区| 久在操| 亚洲精品无码久久久久y| 亚洲激情综合| 玩50岁四川熟女大白屁股直播| 欧洲精品欧美精品| 国产成人亚洲精品| 亚洲精品日韩一区二区电影| 深爱婷婷网| 国产精品免费视频网站| 狠狠干干干| 国产顶级熟妇高潮xxxxx| 精品深夜av无码一区二区| 亚洲男女免费视频| 久久天天躁狠狠躁夜夜av| 中字无码av电影在线观看网站 | 婷婷久久综合| 日韩激情无码免费毛片| 日产2021免费一二三四区在线| 亚洲a∨无码男人的天堂| 欧洲美熟女乱av亚洲一区| 又爽又黄禁片视频1000免费| 无码人妻丰满熟妇区免费| 扒开双腿猛进入喷水高潮叫声| 四川老熟女下面又黑又肥| 亚洲av永久无码精品| 久久精品美女久久| 红桃av一区二区三区在线无码av| 西西人体大胆瓣开下部自慰| 一级做a爰片久久毛片看看| 成年女人毛片免费视频| a级毛片免费完整视频| 加勒比啪啪| 欧洲美熟女乱又伦av影片| 国产女人和拘做受视频免费|